The effects of surface conditioning and aging on the bond strength between composite cement and zirconia-reinforced lithium-silicate glass-ceramics
PURPOSE: To determine the effects of ceramic-surface conditioning and aging on the bond strength between composite cement and zirconia-reinforced lithium-silicate glass-ceramics (ZLS) under simulated clinical conditions. - MATERIALS AND METHODS: ZLS disks (Celtra Duo, Dentsply Sirona, n = 110 test g...
Saved in:
| Main Authors: | , , , |
|---|---|
| Format: | Article (Journal) |
| Language: | English |
| Published: |
2019
|
| In: |
The journal of adhesive dentistry
Year: 2019, Volume: 21, Issue: 6, Pages: 567-576 |
| ISSN: | 1757-9988 |
| DOI: | 10.3290/j.jad.a43650 |
| Online Access: | Resolving-System, Volltext: http://doi.org/10.3290/j.jad.a43650 |
| Author Notes: | Wolfgang Bömicke, Peter Rammelsberg, Johannes Krisam, Stefan Rues |
MARC
| LEADER | 00000caa a2200000 c 4500 | ||
|---|---|---|---|
| 001 | 1689569239 | ||
| 003 | DE-627 | ||
| 005 | 20220817223252.0 | ||
| 007 | cr uuu---uuuuu | ||
| 008 | 200206s2019 xx |||||o 00| ||eng c | ||
| 024 | 7 | |a 10.3290/j.jad.a43650 |2 doi | |
| 035 | |a (DE-627)1689569239 | ||
| 035 | |a (DE-599)KXP1689569239 | ||
| 035 | |a (OCoLC)1341303712 | ||
| 040 | |a DE-627 |b ger |c DE-627 |e rda | ||
| 041 | |a eng | ||
| 084 | |a 33 |2 sdnb | ||
| 100 | 1 | |a Bömicke, Wolfgang |d 1981- |e VerfasserIn |0 (DE-588)1015022146 |0 (DE-627)668338792 |0 (DE-576)349947651 |4 aut | |
| 245 | 1 | 4 | |a The effects of surface conditioning and aging on the bond strength between composite cement and zirconia-reinforced lithium-silicate glass-ceramics |c Wolfgang Bömicke, Peter Rammelsberg, Johannes Krisam, Stefan Rues |
| 264 | 1 | |c 2019 | |
| 300 | |a 10 | ||
| 336 | |a Text |b txt |2 rdacontent | ||
| 337 | |a Computermedien |b c |2 rdamedia | ||
| 338 | |a Online-Ressource |b cr |2 rdacarrier | ||
| 500 | |a Gesehen am 06.02.2020 | ||
| 520 | |a PURPOSE: To determine the effects of ceramic-surface conditioning and aging on the bond strength between composite cement and zirconia-reinforced lithium-silicate glass-ceramics (ZLS) under simulated clinical conditions. - MATERIALS AND METHODS: ZLS disks (Celtra Duo, Dentsply Sirona, n = 110 test group n = 10, diameter: 8.3 mm, height: 3.4 mm) were assigned to four surface-conditioning groups: (I) 30 s of ~5% hydrofluoric-acid etching (Vita Ceramics Etch, Vita; HF), silanization (Calibra Silane; SIL); (II) successive contamination with saliva and silicone (CONT), HF, SIL; (III) CONT, tribochemical silicatization (CoJet), SIL; (IV) HF, SIL, application and light polymerization of an adhesive (Prime&Bond Active), CONT, reapplication and light polymerization of the adhesive. The ZLS disks were bonded to composite-resin cylinders in acrylic tubes (inner diameter: 3.3 mm) using self-adhesive composite cement (Calibra Universal). The tensile-bond strength (TBS) was measured after both 24 h and 6 months of water storage (WS). Additional aging protocols were tested for group I (3-day WS; 30-day WS including 7500 thermocycles between 6.5 and 60°C; 150-day WS including 37,500 thermocycles). - RESULTS: After 24 h, the mean TBS ranged between 21 MPa (group III) and 30-35 MPa (remaining groups). With the exception of 3-day WS, TBS was statistically significantly reduced by aging. The greatest reduction was observed for silicatized specimens (group III, mean TBS after aging: 9.8 MPa). - CONCLUSION: Both ceramic surface conditioning and aging had a statistically significant effect on the bond strength between composite cement and ZLS. A treatment protocol based on tribochemical silicatization cannot be recommended for the adhesive cementation of ZLS. | ||
| 650 | 4 | |a acid etching | |
| 650 | 4 | |a adhesive cementation | |
| 650 | 4 | |a aging | |
| 650 | 4 | |a air abrasion | |
| 650 | 4 | |a all-ceramic | |
| 650 | 4 | |a bond durability | |
| 650 | 4 | |a Ceramics | |
| 650 | 4 | |a composite cement | |
| 650 | 4 | |a Composite Resins | |
| 650 | 4 | |a Dental Bonding | |
| 650 | 4 | |a Dental Porcelain | |
| 650 | 4 | |a Lithium | |
| 650 | 4 | |a Materials Testing | |
| 650 | 4 | |a Resin Cements | |
| 650 | 4 | |a Silanes | |
| 650 | 4 | |a Silicates | |
| 650 | 4 | |a Surface Properties | |
| 650 | 4 | |a tensile bond strength | |
| 650 | 4 | |a Tensile Strength | |
| 650 | 4 | |a Zirconium | |
| 700 | 1 | |a Rammelsberg, Peter |d 1959- |e VerfasserIn |0 (DE-588)122469836 |0 (DE-627)705920836 |0 (DE-576)293285640 |4 aut | |
| 700 | 1 | |a Krisam, Johannes |d 1986- |e VerfasserIn |0 (DE-588)1016031343 |0 (DE-627)705475034 |0 (DE-576)351438696 |4 aut | |
| 700 | 1 | |a Rues, Stefan |e VerfasserIn |0 (DE-588)1054444927 |0 (DE-627)792098331 |0 (DE-576)410292168 |4 aut | |
| 773 | 0 | 8 | |i Enthalten in |t The journal of adhesive dentistry |d Berlin : Quintessence Verlags-GmbH, 1999 |g 21(2019), 6, Seite 567-576 |h Online-Ressource |w (DE-627)363778284 |w (DE-600)2109518-8 |w (DE-576)114670897 |x 1757-9988 |7 nnas |a The effects of surface conditioning and aging on the bond strength between composite cement and zirconia-reinforced lithium-silicate glass-ceramics |
| 773 | 1 | 8 | |g volume:21 |g year:2019 |g number:6 |g pages:567-576 |g extent:10 |a The effects of surface conditioning and aging on the bond strength between composite cement and zirconia-reinforced lithium-silicate glass-ceramics |
| 856 | 4 | 0 | |u http://doi.org/10.3290/j.jad.a43650 |x Resolving-System |3 Volltext |
| 951 | |a AR | ||
| 992 | |a 20200206 | ||
| 993 | |a Article | ||
| 994 | |a 2019 | ||
| 998 | |g 1054444927 |a Rues, Stefan |m 1054444927:Rues, Stefan |d 910000 |d 910800 |e 910000PR1054444927 |e 910800PR1054444927 |k 0/910000/ |k 1/910000/910800/ |p 4 |y j | ||
| 998 | |g 1016031343 |a Krisam, Johannes |m 1016031343:Krisam, Johannes |d 910000 |d 999701 |e 910000PK1016031343 |e 999701PK1016031343 |k 0/910000/ |k 1/910000/999701/ |p 3 | ||
| 998 | |g 122469836 |a Rammelsberg, Peter |m 122469836:Rammelsberg, Peter |d 910000 |d 910800 |e 910000PR122469836 |e 910800PR122469836 |k 0/910000/ |k 1/910000/910800/ |p 2 | ||
| 998 | |g 1015022146 |a Bömicke, Wolfgang |m 1015022146:Bömicke, Wolfgang |d 910000 |d 910800 |e 910000PB1015022146 |e 910800PB1015022146 |k 0/910000/ |k 1/910000/910800/ |p 1 |x j | ||
| 999 | |a KXP-PPN1689569239 |e 3588687769 | ||
| BIB | |a Y | ||
| SER | |a journal | ||
| JSO | |a {"id":{"doi":["10.3290/j.jad.a43650"],"eki":["1689569239"]},"recId":"1689569239","name":{"displayForm":["Wolfgang Bömicke, Peter Rammelsberg, Johannes Krisam, Stefan Rues"]},"type":{"media":"Online-Ressource","bibl":"article-journal"},"person":[{"role":"aut","roleDisplay":"VerfasserIn","given":"Wolfgang","display":"Bömicke, Wolfgang","family":"Bömicke"},{"roleDisplay":"VerfasserIn","given":"Peter","display":"Rammelsberg, Peter","family":"Rammelsberg","role":"aut"},{"roleDisplay":"VerfasserIn","display":"Krisam, Johannes","given":"Johannes","family":"Krisam","role":"aut"},{"role":"aut","roleDisplay":"VerfasserIn","given":"Stefan","display":"Rues, Stefan","family":"Rues"}],"title":[{"title":"The effects of surface conditioning and aging on the bond strength between composite cement and zirconia-reinforced lithium-silicate glass-ceramics","title_sort":"effects of surface conditioning and aging on the bond strength between composite cement and zirconia-reinforced lithium-silicate glass-ceramics"}],"origin":[{"dateIssuedKey":"2019","dateIssuedDisp":"2019"}],"note":["Gesehen am 06.02.2020"],"physDesc":[{"extent":"10 S."}],"relHost":[{"pubHistory":["1.1999 -"],"id":{"issn":["1757-9988"],"zdb":["2109518-8"],"eki":["363778284"]},"recId":"363778284","title":[{"title_sort":"journal of adhesive dentistry","title":"The journal of adhesive dentistry"}],"type":{"bibl":"periodical","media":"Online-Ressource"},"part":{"volume":"21","text":"21(2019), 6, Seite 567-576","extent":"10","year":"2019","pages":"567-576","issue":"6"},"corporate":[{"display":"International Academy for Adhesive Dentistry","roleDisplay":"Herausgebendes Organ","role":"isb"}],"origin":[{"dateIssuedDisp":"[1999]-","publisher":"Quintessence Verlags-GmbH","publisherPlace":"Berlin"}],"language":["eng"],"disp":"The effects of surface conditioning and aging on the bond strength between composite cement and zirconia-reinforced lithium-silicate glass-ceramicsThe journal of adhesive dentistry","physDesc":[{"extent":"Online-Ressource"}],"note":["Gesehen am 29.7.2023","Fortsetzung der Druck-Ausgabe"]}],"language":["eng"]} | ||
| SRT | |a BOEMICKEWOEFFECTSOFS2019 | ||